Recently we reported that the ceramics made of composite BST (Ba0.6Sr0.4TiO3) material have an extremely high tunability of relative permittivity when changing the ceramic temperature; and by cooling the ceramics to 14-15 °C, they provided the best improvement for 17O MRSI application at 10.5T, resulting in an optimal permittivity of ~6000. In this study, we developed new ceramic disks made of mixed Ba0.6Sr0.4TiO3 and BaTiO3 (BST-BT) materials to achieve the optimal permittivity at room temperature. The results indicate that unprecedented performance is possible for 17O MRSI application at 10.5T without the need of a temperature controller.